Low Temperature Differential Scanning Calorimeter 0.001mW

Categories DSC Differential Scanning Calorimeter
Atmosphere control: automatic instrument switching
Gas pressure: 0.2MPa
DSC noise: 0.001 mW
Heating rate: 0.1~80℃/m
Parameter standard: Equipped with standard materials, with one-key calibration function, users can calibrate temperature and enthalpy by themselves
Data interface: standard USB interface
Brand Name: BAXIT
Model Number: BXT-DSC100L
Certification: CE
Place of Origin: China
MOQ: 1
Payment Terms: L/C,T/T,D/A,Western Union
Supply Ability: 1000units
Delivery Time: 3 working days
Packaging Details: wooden
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Low Temperature Differential Scanning Calorimeter 0.001mW

BAXIT DSC low temperature differential scanning calorimetry



Overview:

Differential scanning calorimeter (heat flow DSC) is a classic thermal analysis method of thermal effects under controllable program temperature. It is used in the research and development, process optimization, quality control and failure analysis of various materials and chemistry fields. It has been widely used in various occasions. Using the DSC method, we can study the phase transition of inorganic materials, the melting of polymer materials, the crystallization process, the polymorphism of drugs, the solid/liquid ratio of foods such as oils and fats.


Technical characteristics:

1, industrial-grade wide-screen touch structure, display information is rich, including set temperature, sample temperature, oxygen flow, nitrogen flow, differential heat signal, various switch states.

2, USB communication interface, strong versatility, reliable signal without interruption, support self-recovery connection function.

3. Perfect two-way atmosphere control system, precise control of purge gas flow, automatic switching of software settings, and data directly recorded in the database.

4. Using Cortex-M3 core ARM controller, the calculation processing speed is faster, and the temperature control is more accurate.

5. Using USB two-way communication, the operation is more convenient and supports self-recovery connection function.

6. The digital gas mass flow meter automatically switches the two-way air flow, and the switching speed is fast and the stabilization time is short.

7. Standard samples are standard to facilitate the customer to correct the temperature coefficient.

8, software adaptive resolution computer screen; support notebook, desktop, support WIN2000, XP, WIN7, WIN8, WIN10 and other operating systems.

9. Support user self-programming program to realize full automation of measurement steps. The software provides dozens of instructions, and the user can flexibly combine the instructions according to their own measurement steps and save them. Complex operations are simplified into one-button operation.

Technical Parameters:

DSC range0 ~ ± 500mW
Temperature range-150 ~ 600 ° C
Heating rate0.1~80°C/min
Temperature resolution0.01 ° C
Temperature accuracy± 0.1 ° C
Temperature repeatability± 0.1 ° C
DSC accuracy± 2%
DSC resolution0.001mW
DSC sensitivity0.001mW
Temperature control modeHeating, constant temperature, cooling, cycle temperature control (full program automatic control)
Curve scanTemperature scan
Atmosphere controlGas mass flow meter automatically switches two gas channels
Display mode24bit color, 7 inch LED touch screen display
Data interfaceUSB standard interface, supporting the corresponding operating software
Parameter standardEquipped with standard calibrator with one-button calibration function, users can calibrate the temperature by themselves
Working powerAC220V 50Hz/60Hz


Applications:

Measure physical and chemical changes related to heat, such as glass transition temperature and melting point. Melting temperature, crystallization and crystallization heat, phase transition heat, product thermal stability, solidification/crosslinking, oxidation induction period, reaction kinetics, specific heat, and the like.

Product Picture:





Buy Low Temperature Differential Scanning Calorimeter 0.001mW at wholesale prices
Send your message to this supplier
 
*From:
*To: Shanghai Glomro Industrial Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0